| Volume Range | 5 - 50 μL |
| Increment | 0.5 μL |
| Test Volume |
50 μL 25 μL 5 μL |
| Accuracy error |
0.60 % 0.90 % 2.00 % |
| Precision error |
0.30 % 0.60 % 2.00 % |
- Autoclavable at 121 °C
- Material: Polycarbonate
- Available in 0.1 µL to 5000 µL volume
- Ergonomic design provides excellent operating experience
- Easy-to-read volume display
- Trouble-free calibration and maintenance