| Temperature range | RT to 600°C (Air cooled) |
| Temperature resolution | 0.1°C |
| Temperature fluctuations | ± 0.1°C |
| Temperature repeatability | ± 0.1°C |
| Dynamic heat flow range (DSC range) | 0 to ± 500 mW |
| Heating rate | 1 to 80°C / min |
| Cooling rate | 1 to 20°C / min |
| DSC noise | 0.01 μW |
| DSC resolution | 0.01 µW |
| DSC accuracy | 0.1 µW |
| DSC sensitivity | 0.1 µW |
| Control Mode | Rising temperature, constant temperature (full automatic) |
| Curve scanning | Rising scan, cooling scan |
| Gas flow control | Embedded digital flow meter & Software control, automatic changing |
| Parameter standard | With standard material, with calibration function, the user may correct temperature and heat enthalpy |
| Display | 24 bit 7 inches LCD touch screen display |
| Data interface | Standard USB connector |
| Power Consumption | Less than 2000 W |
| Packaging Dimension and Gross weight (2 case) |
580×490×520 mm / 29 kg 530×270×280 mm / 15 kg |
- Renewed design of oven structure
- High stability and resolution of base line
- Accurate control of air flow rate
- Test data storage function
- Both main frame and software control option
- LCD touch screen display
- Meets ISO and ASTM standards
It is used to study thermal transitions, heat capacity, glass transition temperature, crystallinity, melting temperature etc. of various materials like polymers, plastics, elastomer, food stuffs, biomolecules, non-corrosive samples, electronic components etc.
| Name of Accessories | Quantity |
| Host instrument | 1 |
| CD | 1 |
| Data Line | 1 |
| Power Line | 1 |
| Aluminium crucibles | 100 |
| Ceramic crucibles | 100 |
| pure tin grains | 1bag |
| Fuse 4A | 5 |
info@laboscience.com 